Most enquiries we receive name a thickness and a width before they name an alloy. That is reasonable, because the three alloys we roll cover a wide range of work and the wrong choice rarely shows up until the material is already on a press or a roll former.
The practical difference between 1060, 1100 and 3003 is strength against formability. Everything else follows from that.
What the designations mean
1060 and 1100 belong to the 1000 series, which is commercially pure aluminium. The metal is soft, forms easily, conducts heat and electricity well, and resists corrosion in ordinary atmospheric conditions.
3003 belongs to the 3000 series, where manganese is added as the main alloying element. Manganese raises strength without giving up much of the formability or the corrosion resistance that makes pure aluminium easy to work with.
1060 and 1100
1060 is the purer of the two. It is the usual choice where the metal has to bend tightly, draw deeply, or carry heat or current, and where the part is not expected to take much load.
1100 carries a small amount of copper and is slightly stronger than 1060 while behaving much the same on the shop floor. Where a job runs well in 1060 but the finished part feels too soft to handle, 1100 is the smaller step to take.
3003
3003 is stronger than either 1000 series alloy and still forms well. It is the common choice for panels that have to stay flat over a span, for pressed and roll formed profiles, and for containers that must hold their shape when handled.
It also takes coating and anodising predictably, which is why our colour coated and anodised lines run a great deal of it.
Side by side
| 1060 | 1100 | 3003 | |
|---|---|---|---|
| Strength | Lowest | Slightly above 1060 | Highest of the three |
| Formability | Best | Close to 1060 | Good, below the 1000 series |
| Thermal and electrical conduction | Best | Close to 1060 | Lower |
| Typical use | Deep drawn parts, heat and current paths | General fabrication where 1060 is too soft | Panels, formed profiles, containers |
How the choice usually gets made
Start from what happens to the metal after it leaves the mill rather than from the alloy table.
- If the part is drawn or bent to a tight radius, the 1000 series is the safer starting point.
- If the part has to stay flat, stay rigid, or survive handling, 3003 is usually where the enquiry ends up.
- If the surface is going to be coated or anodised, say so early. It affects the substrate choice as much as the mechanical requirement does.
- Temper matters as much as alloy. An annealed 3003 sheet forms more easily than a hard rolled 1060 one.
We roll all three in sheet and coil from 0.2 to 3.0 mm and in foil from 0.02 to 0.2 mm, in widths from 200 to 1333 mm, slit to order. If the specification is still open, send the part drawing or a description of the forming step and we will say which of the three we would run.
Minimum order is 1 MT for standard specifications and 6 MT for custom ones.