O, H24 and H18: What Temper Changes

Alloy and thickness are usually the first two things an enquiry specifies. Temper is the field most often left blank, and it is the one that decides whether the material cracks at the first bend or springs back out of tolerance.

Two coils of the same alloy at the same gauge can behave nothing alike. What separates them is how much cold work is left in the metal when it ships.

O, H24 and H18: What Temper Changes

Where temper comes from

Cold rolling hardens aluminium. Every pass makes the metal stronger and less willing to stretch. Annealing reverses it: the coil is held at temperature until the structure recrystallises, and it comes out soft again.

A temper designation records where the material sits between those two states. O is fully annealed. H18 is fully hard, rolled down with no annealing afterwards. H24 sits in between, cold worked and then partially annealed back.

What each one is good for

TemperStateBehaves likeCommon work
OFully annealedSoft, stretches furthest before it tearsDeep drawing, tight radius bends, container forming
H24Half hard, partially annealedHolds a shape but still bends without crackingRoll forming, profiles, panels that are worked then installed
H18Fully hardStiff and flat, little left in it to formFlat panels, cladding, work that is cut rather than formed

The failures to expect

Most temper problems show up in one of three ways, and all three are visible in the first few parts off the line.

  • Cracking at a bend or a draw corner usually means the material is too hard for the radius. A softer temper, or a larger radius, is the fix.
  • Springback that puts the part out of tolerance points the same way: the metal is holding more strength than the tooling was set for.
  • Parts that dent or lose shape in handling generally mean the temper is too soft for the job, not that the alloy was wrong.
  • Coil set and edge wave are flatness questions rather than temper ones, though a hard temper makes them harder to correct downstream.

What to send with an enquiry

If the temper is not fixed by a drawing or a standard, the useful thing to describe is the forming step: the tightest bend radius, the draw depth, or whether the sheet is simply cut and fixed. That is enough to decide between the three in most cases.

We anneal to O, H24 and H18 on 1060, 1100 and 3003, in sheet and coil from 0.2 to 3.0 mm and in foil from 0.02 to 0.2 mm. Widths run from 200 to 1333 mm, slit to order.